Welcome to R.K. Laboratory & Scientific Instrument
Ink Decolorization Testing Machine
Instrument installation: The color printed product or finished product containing ink should be placed for 24 hours before testing. After cutting to a width of 60mm×210mm, it is fixed on the friction table, and the surface of the test article cannot afford to be unclean. Experiment procedure: After removing the upper friction body, the length and width of the white doline paper of 50 mm×200 mm were taken and fixed on the upper friction body (on the black rubber body). 1. the sample to be tested is fixed on the lower friction table in four steps.Second, the upper part of the paper wrapped with white wood is rubbed and fixed on the transmission arm, and the weight is set again. Open the calculator box and set the number of frictions. The friction speed is (21/42/85/106 times/minutes adjustable). 2. press the 0N/OFF switch, the number of friction can be automatically shut down for a set number of times.